Technical Parameters | ||||
Properties | Unit | Standard Value | Testing Method | |
Gram weight | g/㎡ | 100(deviations 0~10) | GB/T 29848-2018 | |
Thickness | mm | 2m内(Tmax - Tmin)≤0.02 | GB/T 29848-2018 | |
Optical Transmission(380-1100nm) | % | ≥91 | ||
Optical Transmission(280-380nm) | % | ≥80 | ||
Degree of crosslinking | % | 70~90 | ||
Degree of pre-crosslinking | % | 45-55 | ||
Peel strength | N/cm | With Cells≥50 | GB/T2790-1995 | |
Tensile strength | Mpa | ≥16 | ISO 527-3 | |
Elongation | % | ≥450 | ||
Max traction force before curing | N | ≥5 | GB/T 2410-2008 | |
Density | G/cm3 | 0.9-0.98 | ISO 1183-1 | |
Volume resistivity | Ω/cm | ≥1015 | GB/T 1410-2006 | |
Breakdown voltage | kV/mm | ≥30 | GB/T 1408.1-2006 | |
Fog degree | % | ≤7 | GB/T 2410-2008 | |
UV Light resistance(200kwh/m²) | △YI | <5.0 | GB/T29848-2018 | |
N/cm | UV aging with cell ≥ 30 | GB/T29848-2018 | ||
Heat/humidity resistance85℃/85RH, 1000h | △YI | <5.0 | GB/T29848-2018 | |
N/cm | UV aging with cell ≥ 30 | GB/T29848-2018 | ||
shrinkage | MD | % | ≤5.0 | |
TD | % | ≤2.5 |